WMS Brochure 2026 Digital Organized - Flipbook - Page 28
Striking
Following annealing, the blanks are generally
subjected to a further cleaning stage. During
heating, a light layer of oxide or scale may
form on the surface of the metal. This must
be removed to prevent imperfections appearing
in the 昀椀nished medal. Cleaning methods vary
depending on the material, but the objective
remains consistent: to produce a smooth, uniform
surface ready for striking. Proper preparation at
this stage is essential to achieving a high-quality
昀椀nal result.
of the dies, taking on the form of the design. The
success of this operation depends on a balance
of factors, including the condition of the blank,
the quality of the dies, and the consistency of the
applied force.
The amount of pressure required varies according
to several factors, including the size of the medal,
the hardness of the metal, and the depth and
complexity of the design. In earlier periods,
striking was performed using screw presses or
drop hammers operated by skilled craftsmen,
where experience and judgement played a key role
in achieving consistent results. Later developments
introduced mechanical and hydraulic presses
capable of delivering controlled and repeatable
pressure at higher speeds, improving ef昀椀ciency
while maintaining accuracy.
With the blanks softened and cleaned, they
are ready for the central operation of medal
manufacture: striking, also known as coining. This
is the stage at which the design is permanently
impressed into the metal. Striking is carried out
using hardened steel dies mounted within a press.
The lower die, often referred to as the anvil die,
carries one side of the design, while the upper die
carries the reverse. Each die is precisely engraved
to ensure that the 昀椀nal impression re昀氀ects the
intended detail and proportions.
For medals featuring particularly deep relief
or intricate detailing, a single strike may not be
suf昀椀cient to achieve the desired result. In such
cases, the process may be repeated, with the medal
undergoing additional strikes to fully develop the
design. Between these stages, the metal may be
annealed again to restore its softness, ensuring
that further impressions can be made without the
risk of cracking, distortion, or loss of detail.
During the process, the annealed blank is carefully
positioned between the dies. The press is then
activated, bringing the upper die down with
considerable force. Under this pressure, the metal
昀氀ows outward and upward into the recessed areas
25